What are the main aspects of injection mold cooling water leakage

Injection mold cooling water leakage is a frequent occurrence, for many reasons, mainly in the following aspects:
The most occurs at the joint of the mold cooling water pipe. If water leakage is found, the sealing tape should be wound around the thread of the pipe joint and then tightened.
2, Due to long-term molding conditions, the waterproof ring inside the mold will be damaged, and the O-shaped waterproof rubber ring will easily harden and crack, resulting in water leakage. Some poorly installed waterproof rings can also cause seal failure. It is generally necessary to regularly check the installation position and sealing performance of the seal.
3, The hole wall of the cooling water hole is broken. This often happens when a new mold is tried. The wall thickness of the design is sufficient, but the hole wall is broken due to machining errors or post-processing. In most cases, leaking water holes can no longer be used.
4, Regularly repair the heating pipe and decompression pump and use. The heating tube is an effective heat transfer element and is very effective for core cooling of deep and deep structures. In the area where the cooling water is easy to pass, a one-way heating pipe is provided to reduce water leakage. In addition, the use of a vacuum pump to pump cooling water is also a method to prevent leakage of cooling water.
5, maintenance of the cooling water hole. It is easy to form scale in the cooling water hole, which hinders heat transfer. In severe cases, the water path is blocked and needs regular maintenance. For straight water holes, an iron bar that is 0.5 mm smaller than the diameter of the cooling water hole can be inserted and tapped with a hammer to remove scale and rust. For the cooling water pipe buried in the mold, the mold should be disassembled to remove rust.
After the inspection, the water leakage test should be carried out. The hand pressure pump is used to fill the water hole with water, and it is kept at a pressure of 2 MPa for 5 minutes. It is judged whether the water hole leaks by observing whether the water pressure is lowered. The water leakage can be blocked by mechanical fastening using elastic materials such as rubber and cork, and the room temperature curing type silica gel can be tried as a sealing material.
2018/08/02 10:11:16 6611 次

Hot News

Copy right of the 2018 Wuxi Funecon Precision Mould Plastic Co., Ltd. All Rights Reserved

潍柴动力控股子公司拟开展融资租赁业务|潍柴动力 “十四五”时期四川文化保护传承成效显著 朱军红:深刻转型催生新机遇,上海钢联将与广大客户携手并进 国务院安委会办公室派出工作组对多地打击盗采矿产资源整治工作进行明查暗访 乌克兰据悉在地中海击中了俄罗斯影子船队的一艘油轮 “瞪羚”挑战“大象”:日本经济背后的企业战争 4.5亿元资金如何盘活百亿元级“沉睡”资产?|房地产 许正宇:明年香港重点发展黄金市场 深化与沪深合作|香港 (机遇香港)香港财库局局长:香港黄金市场全产业链已初步形成 “生育友好宫颈健康关爱行动”公益项目在京启动 广西国资拟入主! 这家公司复牌涨停|广西 中关村科技租赁就铜箔生产设备订立融资租赁协议|中关村科技租赁 “港股GPU第一股”壁仞科技确定IPO发售价格区间,预计明年1月2日上市交易|gpu 中国游戏产业聚焦“上海时间” 真金白银培育次世代消费生态|上海市 卓然股份(688121)被证监会立案调查,受损股民可索赔 百大集团换手率23.96%,上榜营业部合计净卖出3015.25万元|百大集团 国家药监局批准盐酸匹米替尼胶囊上市 光峰科技荣膺“金曙光ESG实践奖”,树立可持续发展新标杆 武进不锈:2026年1月7日召开2026年第一次临时股东会|武进不锈 浦发银行获批收购巩义浦发村镇银行并设立分支机构 流水上亿小微被“小钱”卡住,分期乐普惠让厂里机器不停转、鱼虾满塘跃 清仓甩卖、货架空空……万宁闭店前夜,谁在抢购“最后的港妆”?